2008, 'Self-discharge behavior of LaNi5-based hydrogen storage electrodes in different electrolytes', Journal of Solid State Electrochemistry, 12, pp. 935 - 940, http://dx.doi.org/10.1007/s10008-008-0517-3
,2007, 'Hydrogen-enhanced cracking of 2205 duplex stainless steel', Fatigue and Fracture of Engineering Materials and Structures, 30, pp. 1228 - 1236, http://dx.doi.org/10.1111/j.1460-2695.2007.01191.x
,2007, 'The effect of short time post-weld heat treatment on the fatigue crack growth of 2205 duplex stainless steel welds', International Journal of Fatigue, 29, pp. 2155 - 2162, http://dx.doi.org/10.1016/j.ijfatigue.2007.01.004
,2007, 'Discharge behavior of MmNi(3.66)(CoAlMn)(1.34) hydrogen storage alloys', Journal of Alloys and Compounds, 438, pp. 298 - 302
,2007, 'Performance improvement of pasted nickel electrodes with multi-wall carbon nanotubes for rechargeable nickel batteries', Electrochimica ACTA, 53, pp. 1890 - 1896
,2007, 'Tensile behaviour of nano-particulate reinforced aluminium matrix composites at elevated temperature', Materials Science Forum, 561-565, pp. 761 - 764
,2006, 'Nanocrystalline nickel hydroxide in pasted nickel electrodes for rechargeable nickel batteries', Proceedings of the 2006 International Conference on Nanoscience and Nanotechnology, ICONN, pp. 127 - 129, http://dx.doi.org/10.1109/ICONN.2006.340567
,2006, 'Effects of ball milling on the physical and electrochemical characteristics of nickel hydroxide powder', Journal of Applied Electrochemistry, 36, pp. 97 - 103
,2006, 'Performance improvement of pasted nickel electrodes with an addition of ball-milled nickel hydroxide powder', Electrochimica ACTA, 51, pp. 6548 - 6555
,2006, 'Review of alloy membranes/film for hydrogen separation or purification', Journal of Rare Earths, 23, pp. 611 - 616
,2006, 'Structural stability of single-layered LaNi4.25Al0.75 film and its electrochemical hydrogen-storage properties', Rare Metals, 25, pp. 543 - 548
,2005, 'Electrocatalysis for hydrogen evolution reaction on nickel-hydrogen storage alloy composite electrodes prepared by electrodeposition', Tianjin Daxue Xuebao (Ziran Kexue yu Gongcheng Jishu Ban)/Journal of Tianjin University Science and Technology, 38, pp. 508 - 512
,2005, 'Effect of nano-scale particles on the creep behavior of 2014 Al', Materials Science and Engineering: A, 394, pp. 103 - 111, http://dx.doi.org/10.1016/j.msea.2004.11.034
,2005, 'Hydrogen-enhanced cracking of 2205 duplex stainless steel welds', Materials Chemistry and Physics, 91, pp. 21 - 27
,2005, 'Physical and electrochemical characteristics of nanostructured nickel hydroxide powder', Journal of Applied Electrochemistry, 35, pp. 157 - 162
,2005, 'Review of alloy membranes/film for hydrogen separation or purification', Journal of Rare Earths, 23, pp. 611 - 616
,2004, 'Effect of temper, specimen orientation and test temperature on tensile and fatigue properties of wrought and PM AA6061-alloys', International Journal of Fatigue, 26, pp. 691 - 703, http://dx.doi.org/10.1016/j.ijfatigue.2003.11.006
,2004, 'Electroless Co-Zn surface-modified nickel hydroxide as an active material for pasted nickel electrodes', Transactions of Tianjin University, 10, pp. 47 - 53
,2004, 'Formation of Mg2Ni nanofibres in a Mg-based Metal Matrix Composite', Philosophical Magazine, 84, pp. 3771 - 3784
,2004, 'Tensile Properties of Nanometric Al2O3 Particulate-reinforced Aluminium Matrix Composites', Materials Chemistry and Physics, 85, pp. 438 - 443
,2003, 'Study of microstructure, mechanical properties, and magnetization process in low carbon steel bars by Barkhausen emission', Materials Science and Engineering: A, 358, pp. 186 - 198, http://dx.doi.org/10.1016/S0921-5093(03)00295-8
,2003, 'Effect of initial microstructure on the creep behavior of TMCP EH36 and SM490C steels', Materials Science and Engineering: A, 344, pp. 288 - 295, http://dx.doi.org/10.1016/S0921-5093(02)00425-2
,2003, 'Formation of Mg-Mg
2002, 'Structural characteristics of nickel hydroxide synthesized by a chemical precipitation route under different pH values', Journal of Power Sources, 112, pp. 428 - 434, http://dx.doi.org/10.1016/S0378-7753(02)00396-8
,2002, 'Effect of microstructural texture on the creep behavior', Journal of Materials Science, 37, pp. 3733 - 3737, http://dx.doi.org/10.1023/A:1016573628007
,2002, 'Effects of fluorination on the hydriding and electrochemical properties of a gas-atomized Zr-based hydrogen storage alloy', Journal of Alloys and Compounds, 330-332, pp. 617 - 621, http://dx.doi.org/10.1016/S0925-8388(01)01457-8
,2001, 'Effect of Ni encapsulation on the properties of Ti-Zr-based hydrogen storage alloys', Journal of Alloys and Compounds, 314, pp. 224 - 231, http://dx.doi.org/10.1016/S0925-8388(00)01193-2
,2001, 'Nondestructive evaluation of carbon contents and microstructures in plain carbon steel bars by Barkhausen emission', IEEE Transactions on Magnetics, 37, pp. 2734 - 2736, http://dx.doi.org/10.1109/20.951290
,2001, 'Sulfide stress corrosion cracking and fatigue crack growth of welded TMCP API 5L X65 pipe-line steel', International Journal of Fatigue, 23, pp. 103 - 113, http://dx.doi.org/10.1016/S0142-1123(00)00081-5
,2000, 'Effect of grain size and second phase particles on the hydrogen occlusivity of iron and steels', Materials Research Innovations, 3, pp. 263 - 270, http://dx.doi.org/10.1007/s100190000043
,1999, 'Corrosion and hydrogen damage resistance of stainless steels in Ni/MHx batteries', Corrosion Science, 41, pp. 1347 - 1358, http://dx.doi.org/10.1016/S0010-938X(98)00189-9
,1999, 'Effect of annealing heat treatment on an atomized AB
1999, 'Hydrogen trapping ability of steels with different microstructures', Journal of the Chinese Institute of Engineers, Transactions of the Chinese Institute of Engineers,Series A/Chung-kuo Kung Ch'eng Hsuch K'an, 22, pp. 43 - 53, http://dx.doi.org/10.1080/02533839.1999.9670440
,1999, 'Study of the performance of Ti-Zr based hydrogen storage alloys', Journal of Power Sources, 77, pp. 159 - 163, http://dx.doi.org/10.1016/S0378-7753(98)00189-X
,1997, 'Hydrogen permeability and diffusivity in amorphous Metglas 2826MB under AC excitation', Journal of Alloys and Compounds, 253-254, pp. 370 - 373, http://dx.doi.org/10.1016/S0925-8388(96)02906-4
,1996, 'Effects of ferrite/pearlite alignment on the hydrogen permeation in a AISI 4130 steel', Materials Letters, 29, pp. 143 - 147, http://dx.doi.org/10.1016/S0167-577X(96)00140-1
,1996, 'Hydrogen enhanced fatigue crack propagation of bainitic and tempered martensitic steels', Corrosion Science, 38, pp. 2049 - 2060, http://dx.doi.org/10.1016/S0010-938X(96)89123-2
,1995, 'Effect of ageing treatment on the microstructures and properties of T-250 laser welds', International Journal of Materials and Product Technology, 10, pp. 132 - 142
,1993, 'Abrasive wear of aged 2014 and 6061 aluminium alloy composites', Journal of Materials Science Letters, 12, pp. 476 - 477, http://dx.doi.org/10.1007/BF00452799
,1992, 'Abrasive wear of powder metallurgy Al alloy 6061-SiC particle composites', Wear, 159, pp. 223 - 231, http://dx.doi.org/10.1016/0043-1648(92)90305-R
,1992, 'Aging behavior of powder metallurgy composite', Scripta Metallurgica et Materiala, 26, pp. 1723 - 1726, http://dx.doi.org/10.1016/0956-716X(92)90541-L
,1992, 'Effect of aging on the sliding abrasive wear of P M 2014 and 6061 Al alloy-SiC particle composites', Materials Letters, 15, pp. 49 - 52, http://dx.doi.org/10.1016/0167-577X(92)90011-8
,1991, 'Hydrogen embrittlement of AISI 4130 steel with an alternate ferrite/pearlite banded structure', Materials Science and Engineering A, 142, pp. 193 - 201, http://dx.doi.org/10.1016/0921-5093(91)90658-A
,1991, 'Effect of cold rolling on the aging kinetics of Al
1991, 'Effect of retained austenite on the hydrogen content and effective diffusivity of martensitic structure', Metallurgical transactions. A, Physical metallurgy and materials science, 22 A, pp. 2579 - 2586, http://dx.doi.org/10.1007/BF02851351
,1991, 'Hydrogen embrittlement of AISI 4130 steel with an alternate ferrite/pearlite banded structure',
,1991, 'Hydrogen embrittlement of AISI 4130 steel with an alternate ferrite/pearlite banded structure', , 142, pp. 193 - 201
,1986, 'Effect of carbon content on hydrogen occlusivity and embrittlement of ferrite–pearlite steels', Materials Science and Technology (United Kingdom), 2, pp. 956 - 962, http://dx.doi.org/10.1179/mst.1986.2.9.956
,1985, 'Hydrogen occlusivity and embrittlement in iron – effect of grain structure and cold work', Materials Science and Technology (United Kingdom), 1, pp. 454 - 460, http://dx.doi.org/10.1179/mst.1985.1.6.454
,1983, 'Evaluation of three different test methods for charging hydrogen into iron', Metals Technology, 10, pp. 464 - 470, http://dx.doi.org/10.1179/030716983803291695
,